內(nèi)墻膩子膠粉起泡的原因及處理方法
來源:http://www.bjtsdc.com 日期:2022-04-07 發(fā)布人:
內(nèi)墻裝修一般情況下都采用普通的內(nèi)墻膩子膠粉扛浸,使用的粘接劑多為羧甲基纖維素CMC和羧基予湖化淀粉膠冲杀,這兩種粘接劑都會和灰鈣、水泥中的堿性物質(zhì)起凝膠反應(yīng)卢历。當(dāng)堿性較高的墻體遇到中性內(nèi)墻膩子膠粉中的水分就會立即產(chǎn)生反應(yīng)出現(xiàn)小氣泡钱反。這是因為膩子所使用的的填充料為重質(zhì)碳酸鈣或滑石粉黑竞,屬中性無強(qiáng)度不耐水。而墻體為水泥或石灰砂漿界面锁右,屬堿性搜痕。所以遇到堿性較高的墻面易產(chǎn)生氣泡。
Ordinary interior wall putty powder is commonly used for interior wall decoration. Most of the adhesives used are carboxymethyl cellulose CMC and carboxyl group as Lake starch glue. These two adhesives react with alkaline substances in gray calcium and cement. When the wall with high alkalinity meets the water in the putty powder of neutral interior wall, it will react immediately and produce small bubbles. This is because the filler used for the putty is heavy calcium carbonate or talc powder, which is neutral, non strength and water-resistant. The wall is cement or lime mortar interface, which is alkaline. Therefore, it is easy to produce bubbles on the wall with high alkalinity.


在每年七八月份梅雨季節(jié)空氣濕度大队趁,內(nèi)墻膩子膠粉界面非常容易吸濕返潮绍撇,它就會與堿性墻面發(fā)生化學(xué)反應(yīng),出現(xiàn)鼓泡松摘、開裂督垮、發(fā)霉、起皮脫落現(xiàn)象乳栈。特別是南方地區(qū)空氣濕度大影啸,起皮脫落現(xiàn)象更為嚴(yán)重。鋼化拋光膩子同樣常常在批刮時會出現(xiàn)起泡現(xiàn)象组伤,原因是所使用的膠粘劑無透氣功能舌恬,比如使用的摻假纖維素HPMC。摻有CMC或含有羧基成分的其他化工產(chǎn)品扭享。
In the plum rain season in July and August every year, the air humidity is high, and the putty rubber powder interface of the inner wall is very easy to absorb moisture and return to moisture. It will have a chemical reaction with the alkaline wall, resulting in bubbling, cracking, mildew, peeling and falling off. Especially in the south, the air humidity is high, and the peeling and falling off phenomenon is more serious. Toughened polishing putty also often bubbles when scraping, because the adhesive used has no air permeability function, such as adulterated cellulose HPMC. Other chemical products mixed with CMC or containing carboxyl groups.
這樣現(xiàn)象發(fā)生的原因:一是返堿墻面。尤其是室內(nèi)水泥現(xiàn)澆頂板為多見匙蚣,原因是在頂板澆注過程中水泥砂漿中堿性物質(zhì)隨水沉淀聚積于頂板與模板之間续膳,水份干燥蒸發(fā)后,室內(nèi)水泥頂板表面就會呈現(xiàn)較高的堿性氣泡收班。二是水泥砂漿墻面較粗糙坟岔,批刮膩子時將氣體封閉在其中釋放出的氣體形成小氣泡。如果出現(xiàn)起泡現(xiàn)象該如何處理呢?內(nèi)墻膩子膠粉廠家為大家總結(jié)了一些處理辦法:
The reasons for this phenomenon: first, return to alkali wall. In particular, the indoor cement cast-in-situ roof is common, because the alkaline substances in the cement mortar precipitate and accumulate between the roof and the formwork with water during the roof pouring process. After the water is dried and evaporated, the surface of the indoor cement roof will show high alkaline bubbles. Second, the cement mortar wall is rough. When applying putty, the gas will be sealed in it, and the released gas will form small bubbles. How to deal with bubbles? The manufacturer of interior wall putty and rubber powder summarized some treatment methods for you:
1摔桦、河南內(nèi)外墻膩子粉廠家建議更換有透氣功能耐堿性膠粉社付,比如使用國標(biāo)纖維素HPMC非標(biāo)純粉,或有透氣功能的速溶樹脂膠粉邻耕。
1. Henan interior and exterior wall putty powder manufacturers recommend replacing alkali resistant rubber powder with air permeability function, such as using national standard cellulose HPMC non-standard pure powder or instant resin rubber powder with air permeability function.
2鸥咖、批膩子膠粉前可用水噴灑在粗糙墻面或罩白灰墻面上,讓氣體提前釋放后在批膩子兄世,即可避免出現(xiàn)起泡現(xiàn)象啼辣。
2. Before applying putty rubber powder, water can be sprayed on the rough wall or covered with lime. After the gas is released in advance, apply putty to avoid foaming.
以上就是為大家介紹的有關(guān)濟(jì)南膩子粉的詳細(xì)介紹,希望對您有所幫助.如果您有什么疑問的話,歡迎聯(lián)系我們.我們將以的態(tài)度,為您提供服務(wù)http://www.bjtsdc.com
The above is the detailed introduction of Jinan putty powder. I hope it will help you If you have any questions, please contact us We will provide you with professional service http://www.bjtsdc.com