外墻膩子粉彈性說明大家了解嗎
來源:http://www.bjtsdc.com 日期:2020-05-25 發(fā)布人:
由于墻體結(jié)構(gòu)受力變形讹蘑,完成外墻裝飾后,經(jīng)常出現(xiàn)裂縫薛训、裂縫。有人認為水泥基外墻膩子粉容易開裂仑氛,只要產(chǎn)品具有高彈性乙埃,就能解決裂縫問題,裂縫的具體情況如下:
Because of the stress deformation of the wall structure, cracks often appear after the completion of the external wall decoration. Some people think that cement-based putty powder for exterior wall is easy to crack. As long as the product has high elasticity, the crack problem can be solved. The specific situation of the crack is as follows:

了解我國建筑史(1)每個人都知道锯岖,建筑質(zhì)量問題是由于設(shè)計介袜、施工、材料、木材米酬、中國古建筑——北京故宮的城墻沛豌,使用彈性外墻膩子粉,現(xiàn)在560年過去了赃额,沒有出現(xiàn)裂縫加派、開裂、脫落墻面革跳芳、滲水等問題叁渣。
To understand the history of architecture in China (1) everyone knows that the quality of architecture is due to the design, construction, materials, wood, the wall of Beijing Imperial Palace, the ancient Chinese architecture, and the use of elastic putty powder for external walls. Now 560 years have passed, there are no cracks, cracks, peeling off wall leather, water seepage and other problems.
而我們所謂的現(xiàn)代高科技產(chǎn)品,如“真石漆”谍潮、“乳膠漆”溯侦、“氟碳漆”、“釉面瓷磚”慷啊、“彈性膩子”况魔、“GS防水材料”等,可以有幾年某扑、幾十年奢赡、幾百年的使用壽命。采用彈性膩子的建筑筐积,在材料和工藝上均可達到故宮博物院的水平掷暇。
And our so-called modern high-tech products, such as "real stone paint", "latex paint", "fluorocarbon paint", "glazed ceramic tile", "elastic putty", "GS waterproof material", can have several years, decades, hundreds of years of service life. The building with elastic putty can reach the level of the Palace Museum in material and technology.
現(xiàn)代建筑工程,包括基礎(chǔ)設(shè)施建設(shè)和裝修珊求,由于施工高峰期层攀,為節(jié)省資金和麻煩,質(zhì)量隱患較多赃阀,是多年以后霎肯,這些隱患依然存在,薄層膩子榛斯,尤其是彈性膩子不能從根本上解決這些問題姿现。
Modern construction engineering, including infrastructure construction and decoration, has many quality hidden dangers due to the peak period of construction, in order to save money and trouble. After many years, these hidden dangers still exist. Thin layer putty, especially elastic putty, cannot fundamentally solve these problems.
彈性膩子的重要技術(shù)指標之一:動態(tài)抗裂性(底部開裂)≥0.1mm, <0.3mm肖抱。
One of the important technical indexes of elastic putty: dynamic crack resistance (bottom crack) ≥ 0.1mm, < 0.3mm.
外墻膩子粉,以滿足這個索引是很容易的,我們添加更多的好的彈性乳液可以做,問題是當乳膠材料數(shù)量越大,影響越大基于水泥的后期強度和穩(wěn)定的膩子,彈性乳膠維持時間是非常有限的。
External wall putty powder is easy to meet this index. We can add more good elastic emulsion to do it. The problem is that the larger the amount of latex material, the greater the impact. The strength of cement and the stable putty, the maintenance time of elastic latex is very limited.
墻體產(chǎn)生裂縫后,可以存在,及其裂紋大小,每,每一小時,24小時不斷變化的,它會隨環(huán)境溫度的變化,濕度和變化,這種變化可以繼續(xù)建筑使用壽命結(jié)束的時候,要選擇質(zhì)量好异旧、靈活性好外墻膩子粉意述。
After the wall cracks, it can exist permanently, and its crack size will change continuously every day, every hour and 24 hours. It will change with the change of ambient temperature, humidity and change. This change can continue to the end of the service life of the building. When the quality and flexibility of the external wall putty powder are good, it is necessary to choose.
以上是濟南膩子粉公司小編為大家介紹的相關(guān)內(nèi)容,想要了解更多內(nèi)容吮蛹,歡迎訪問網(wǎng)站:http://www.bjtsdc.com
The above is the relevant content introduced by Jinan putty powder company. If you want to know more, please visit the website: http://www.bjtsdc.com